Application description

     Nano-polymer operation manual

 

[component]

 

   The formations of Nano-polymer are consisted of polymer A and polymer B

   1. The component of polymer A are constituted of specific carbon A mixture and related

       ingredients

   2. The component of polymer B are constituted of specific carbon B mixture and related

       ingredients

 

[use]  The usage of Nano-polymer are suggested to be used at water diluent, not suggested

               to use at the powder type to prevent the incorrect trans-purifying purification reaction

 

[preparation]  before usage, the polymer A and polymer B of Nano-polymer are needed to

                                be diluted into water diluent primarily

 

   1. The preparation of polymer A diluents

        polymer A powder   +    clear water       =    polymer A diluents

         1 kg powder                     10 liters                 10 liters A diluents

 

   2. The preparation of polymer B diluents

        polymer B powder   +    clear water       =    polymer B diluents

         1 kg powder                    10 liters                  10 liters B diluents

 

   [Remarks] a. The polymer A/B diluent can be used immediatedly, more better at after 2~3

                         hours preparations

                     b. The polymer A/B diluent are suggested to be usage within 3~7 days

 

[operation]

   1. The purification dosage operation

  Dosage

 

 Polymer A diluent + Polymer A diluent

 

 Treated volumes

300 ppm

(high dosage)

   1 liter A diluent + 1 liter B diluent

0.35 tons

(350 liters)

200 ppm

(high dosage)

   1 liter A diluent + 1 liter B diluent

0.5 tons

(500 liters)

100 ppm

(low dosage)

   1 liter A diluent + 1 liter B diluent

1 tons

(1000 liters)

50 ppm

(low dosage)

   1 liter A diluent + 1 liter B diluent

2 tons

(2000 liters)

10 ppm

(low dosage)

   1 liter A diluent + 1 liter B diluent

10 tons

(10000 liters)

 

   1. The operation procedure ----example: 100 ppm dosage application

        a. step 1:  add 100 ppm polymer A diluents into the treated water, wastewater firstly,

                         and mixing 1~2 minutes

        b. step 2:  add 100 ppm polymer B diluents into the step 1 mixing treated water, waste

                         water, and mixing 1~2 minutes

        c. step 3:  stand the reactive treated water, wastewater to sedimentation, and inspect

                        the purification effect after 10~30 minutes, 1~3 hours, 1~3 days reaction

      Polymer A diluent   mixing                   Polymer B diluent        mixing                       precipitation

       1 liter                     1~2 minutes               1 liter                      1~2 minutes              10~30 minutes

                                                                                                                                               1~3 hours/days

                                                                                                                                              check the result

 

                                                   

 

 

  

 

1

水質污

 

  

 

 

 

 

 

   

 

 

 

 

 

  

   

       
 
 

 

 

 

   

 

 

 

 

                

    1 tons water/wastewater  

 

 

Bright Glory enterprise,Co.Ltd/

SanDa membrane & Nano,Co.Ltd

5F-3, No.162, Sec. 4, Chunghsiao E. Road, Taipei, Taiwan          

Tel: 886-02-2731-8306        Fax: 886-02-2731-8221   

web site: www.bge.com.tw  web site: http://3w.bge.com.tw     Email: hong@bge.com.tw

 

2003.11.25 copy right